TEBAK Slideway Materials

Guides / Installation Guide

Installation Guide

Butt Joints in Long Liner Runs: Where to Place Them

A bed longer than the roll is not one strip, it is several joined end to end. The cut gets the attention; the position of the seam is what decides whether the way still measures flat a year later.

Rolls arrive in 5 to 20 m lengths, so any guideway longer than that is joined. The seam is the only place on the finished way where two surfaces that must behave as one are actually two, and it is the first place a rebuild shows its quality. Placement is settled on the drawing, not at the saw.

Placement rules that survive service

  • Keep the joint out of the working band. A strip wears where the carriage works, not where it parks; a seam under heavy traffic becomes a step on both sides.
  • Never put a seam on the oil groove line. A joint crossing the groove gives oil a way out and grit a way in.
  • Keep it clear of wipers and end stops, which cross the weakest edge twice per stroke.
  • Stagger the joints across the pair, so no cross section carries two seams and the saddle has no rocking line.
Plan view of liner piece A on the left and piece B on the right butted at a single seam across the strip, with the dashed oil groove line running lengthwise below the seam and not crossing it
One seam, one groove: the joint runs across the strip clear of the groove line, so the channel stays continuous and the seam is not a leak path.

Cutting and seating the seam

Cut against a straight edge and check the cut with a square on both the face and the edge. A cut that is out of square looks fine while the piece is loose and shows the moment the second piece is butted against it, as a wedge of daylight no adhesive will close. Recut rather than fill; adhesive is not a shim.

Butt the ends tight, tape the seam before the strip goes down, and work adhesive out from under it instead of letting it pool. A cured bead standing proud of the liner is a ridge that scrapes the mating face at every reversal, and it is the most common reason a well-bonded joint still marks the way.

After cure, scrape the seam flush with the surrounding surface and check it in the same blueing pass as the rest of the face. Contact that stops at the seam means the joint is low; contact that doubles means it is high. Both are joint faults, not flatness faults, and both are cheaper to fix before assembly. The clearance figures that follow come from the routine in gib strip relining.

What a bad joint looks like in service

  • Oil weeping along the seam with the wiper dry on one side: the seam has opened into the groove.
  • A polished step on the mating face, sharp at one edge and blended at the other: the joint stands proud and is hammered at reversal.
  • A rust line under the seam on cast iron: moisture sat in the joint because the cut ends were never sealed.
  • Lifted corners either side of the seam: the pieces were worked after the film had skinned.
  • A single click per reversal: two faces meeting at slightly different heights, load crossing between them.

Where the joint should fall instead

Put it where the machine does not work: at the tail end beyond the usual stroke, outside the wiper track, clear of groove crossings, staggered against the opposite face. On a rebuilt bed the order matters as much as the position, because the seam has to be judged against a surface already ground and measured — the sequence in rebuild sequence.

If the bed needs more than two pieces, hold every seam to the same standard rather than accepting one good joint and one compromise. A single proud seam marks the mating face, and the mark does not stay local to the joint.

Width changes the margin. A 100 mm strip leaves less either side of a seam to carry load than a 305 mm strip, and gives less room to move the joint off a groove. 1.6 mm sheet and 2.0 mm sheet come in the widths the layout calls for, so the seam lands where it belongs rather than where the stock ends.

Ask about a liner specification